Porosity in/on parts
For wall thickness <0.5mm, bubbles form due to poor flow.
For 0.4mm walls, increase light intensity or print time.
For suction-cup shapes, oxygen overflow causes pores; increase print time. Add vent holes to allow flow.
诚一信统一售后平台 · 技术文档For wall thickness <0.5mm, bubbles form due to poor flow.
For 0.4mm walls, increase light intensity or print time.
For suction-cup shapes, oxygen overflow causes pores; increase print time. Add vent holes to allow flow.